{"product_id":"latheland-range-st22-miniature-torus-end-mill-with-long-neck-for-stainless-titanium-superalloys-2-4-flutes","title":"LATHELAND® Miniature Torus End Mill with Long Neck for Stainless, Titanium \u0026 Superalloys, 2\/4 Flutes – ST22","description":"\u003cp\u003eStainless, titanium \u0026amp; superalloys: Variable-helix, chip-breaker and roughing end mills that resist chatter in tough, sticky materials.\u003c\/p\u003e\u003cdiv style=\"border:1px solid #dadada;border-radius:6px;padding:12px 14px;margin:0 0 14px;background:#f8f8f8\"\u003e\u003cp style=\"margin:0\"\u003e\u003cstrong\u003ePrice on request.\u003c\/strong\u003e This tool is part of the LATHELAND full range and is supplied on quotation. Choose the size and send the quote form, or email \u003ca href=\"mailto:info@latheland.com\"\u003einfo@latheland.com\u003c\/a\u003e with the SKU and quantity. We reply with price and delivery time, usually within one working day.\u003c\/p\u003e\u003c\/div\u003e\u003ch4\u003eSpecifications\u003c\/h4\u003e\u003ctable\u003e\n\u003ctr\u003e\n\u003ctd\u003e\u003cstrong\u003eSeries\u003c\/strong\u003e\u003c\/td\u003e\n\u003ctd\u003eST22\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003e\u003cstrong\u003eMaterial\u003c\/strong\u003e\u003c\/td\u003e\n\u003ctd\u003eSolid carbide\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003e\u003cstrong\u003eCoating\u003c\/strong\u003e\u003c\/td\u003e\n\u003ctd\u003eAlCrN \/ Uncoated, polished\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003e\u003cstrong\u003eFlutes\u003c\/strong\u003e\u003c\/td\u003e\n\u003ctd\u003e2\/4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003e\u003cstrong\u003eHelix angle\u003c\/strong\u003e\u003c\/td\u003e\n\u003ctd\u003e40°\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003e\u003cstrong\u003eWorkpiece hardness\u003c\/strong\u003e\u003c\/td\u003e\n\u003ctd\u003eup to 45 HRC\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003e\u003cstrong\u003eBest for\u003c\/strong\u003e\u003c\/td\u003e\n\u003ctd\u003esteel, stainless steel, cast iron, titanium \u0026amp; superalloys\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003e\u003cstrong\u003eRange\u003c\/strong\u003e\u003c\/td\u003e\n\u003ctd\u003eØ0.2–4 mm\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003e\u003cstrong\u003eSizes available\u003c\/strong\u003e\u003c\/td\u003e\n\u003ctd\u003e146\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003e\u003cstrong\u003ePrice\u003c\/strong\u003e\u003c\/td\u003e\n\u003ctd\u003eOn request – supplied on quotation\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003c\/table\u003e\u003ch4\u003eVersions\u003c\/h4\u003e\u003ctable\u003e\n\u003ctr\u003e\n\u003cth\u003eVersion\u003c\/th\u003e\n\u003cth\u003eSpecification\u003c\/th\u003e\n\u003cth\u003eSizes\u003c\/th\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003e\u003cstrong\u003eST22C\u003c\/strong\u003e\u003c\/td\u003e\n\u003ctd\u003eAlCrN\u003c\/td\u003e\n\u003ctd\u003e134\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003e\u003cstrong\u003eST22U\u003c\/strong\u003e\u003c\/td\u003e\n\u003ctd\u003eUncoated, polished\u003c\/td\u003e\n\u003ctd\u003e12\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003c\/table\u003e\u003ch4\u003eSize table (all dimensions in mm)\u003c\/h4\u003e\u003cdiv style=\"overflow-x:auto\"\u003e\u003ctable\u003e\n\u003ctr\u003e\n\u003cth\u003eSKU\u003c\/th\u003e\n\u003cth\u003eØ D\u003c\/th\u003e\n\u003cth\u003eR\u003c\/th\u003e\n\u003cth\u003el1\u003c\/th\u003e\n\u003cth\u003el2\u003c\/th\u003e\n\u003cth\u003eL\u003c\/th\u003e\n\u003cth\u003ed1\u003c\/th\u003e\n\u003cth\u003ed2\u003c\/th\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.2x50\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e0.05\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.17\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.2x50N0.5\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e0.05\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e0.5\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.17\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.2x50N1\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e0.05\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e1\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.17\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.2x50N1.5\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e0.05\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.17\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.3x50\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e0.05\u003c\/td\u003e\n\u003ctd\u003e0.4\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.27\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.3x50N1\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e0.05\u003c\/td\u003e\n\u003ctd\u003e0.4\u003c\/td\u003e\n\u003ctd\u003e1\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.27\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.3x50N2\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e0.05\u003c\/td\u003e\n\u003ctd\u003e0.4\u003c\/td\u003e\n\u003ctd\u003e2\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.27\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.3x50N3\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e0.05\u003c\/td\u003e\n\u003ctd\u003e0.4\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.27\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.4x50\u003c\/td\u003e\n\u003ctd\u003e0.4\u003c\/td\u003e\n\u003ctd\u003e0.05\u003c\/td\u003e\n\u003ctd\u003e0.6\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.37\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.4x50N2\u003c\/td\u003e\n\u003ctd\u003e0.4\u003c\/td\u003e\n\u003ctd\u003e0.05\u003c\/td\u003e\n\u003ctd\u003e0.6\u003c\/td\u003e\n\u003ctd\u003e2\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.37\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.4x50N3\u003c\/td\u003e\n\u003ctd\u003e0.4\u003c\/td\u003e\n\u003ctd\u003e0.05\u003c\/td\u003e\n\u003ctd\u003e0.6\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.37\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.4x50N4\u003c\/td\u003e\n\u003ctd\u003e0.4\u003c\/td\u003e\n\u003ctd\u003e0.05\u003c\/td\u003e\n\u003ctd\u003e0.6\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.37\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.4x50N5\u003c\/td\u003e\n\u003ctd\u003e0.4\u003c\/td\u003e\n\u003ctd\u003e0.05\u003c\/td\u003e\n\u003ctd\u003e0.6\u003c\/td\u003e\n\u003ctd\u003e5\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.37\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.5x50\u003c\/td\u003e\n\u003ctd\u003e0.5\u003c\/td\u003e\n\u003ctd\u003e0.05\u003c\/td\u003e\n\u003ctd\u003e0.7\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.45\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.5x50N2\u003c\/td\u003e\n\u003ctd\u003e0.5\u003c\/td\u003e\n\u003ctd\u003e0.05\u003c\/td\u003e\n\u003ctd\u003e0.7\u003c\/td\u003e\n\u003ctd\u003e2\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.45\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.5x50N4\u003c\/td\u003e\n\u003ctd\u003e0.5\u003c\/td\u003e\n\u003ctd\u003e0.05\u003c\/td\u003e\n\u003ctd\u003e0.7\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.45\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.5x50N6\u003c\/td\u003e\n\u003ctd\u003e0.5\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.5x50N8\u003c\/td\u003e\n\u003ctd\u003e0.5\u003c\/td\u003e\n\u003ctd\u003e0.05\u003c\/td\u003e\n\u003ctd\u003e0.7\u003c\/td\u003e\n\u003ctd\u003e8\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.45\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.6x50\u003c\/td\u003e\n\u003ctd\u003e0.6\u003c\/td\u003e\n\u003ctd\u003e0.05\u003c\/td\u003e\n\u003ctd\u003e0.9\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.55\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.6x50N2\u003c\/td\u003e\n\u003ctd\u003e0.6\u003c\/td\u003e\n\u003ctd\u003e0.05\u003c\/td\u003e\n\u003ctd\u003e0.9\u003c\/td\u003e\n\u003ctd\u003e2\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.55\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.6x50N4\u003c\/td\u003e\n\u003ctd\u003e0.6\u003c\/td\u003e\n\u003ctd\u003e0.05\u003c\/td\u003e\n\u003ctd\u003e0.9\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.55\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.6x50N6\u003c\/td\u003e\n\u003ctd\u003e0.6\u003c\/td\u003e\n\u003ctd\u003e0.05\u003c\/td\u003e\n\u003ctd\u003e0.9\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.55\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.6x50N8\u003c\/td\u003e\n\u003ctd\u003e0.6\u003c\/td\u003e\n\u003ctd\u003e0.05\u003c\/td\u003e\n\u003ctd\u003e0.9\u003c\/td\u003e\n\u003ctd\u003e8\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.55\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.6x50N10\u003c\/td\u003e\n\u003ctd\u003e0.6\u003c\/td\u003e\n\u003ctd\u003e0.05\u003c\/td\u003e\n\u003ctd\u003e0.9\u003c\/td\u003e\n\u003ctd\u003e10\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.55\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.7x50\u003c\/td\u003e\n\u003ctd\u003e0.7\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e1\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.65\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.7x50N2\u003c\/td\u003e\n\u003ctd\u003e0.7\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e1\u003c\/td\u003e\n\u003ctd\u003e2\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.65\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.7x50N4\u003c\/td\u003e\n\u003ctd\u003e0.7\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e1\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.65\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.7x50N6\u003c\/td\u003e\n\u003ctd\u003e0.7\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e1\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.65\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.7x50N8\u003c\/td\u003e\n\u003ctd\u003e0.7\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e1\u003c\/td\u003e\n\u003ctd\u003e8\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.65\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.7x50N10\u003c\/td\u003e\n\u003ctd\u003e0.7\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e1\u003c\/td\u003e\n\u003ctd\u003e10\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.65\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.8x50\u003c\/td\u003e\n\u003ctd\u003e0.8\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e1.2\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.75\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.8x50N4\u003c\/td\u003e\n\u003ctd\u003e0.8\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e1.2\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.75\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.8x50N6\u003c\/td\u003e\n\u003ctd\u003e0.8\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e1.2\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.75\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.8x50N8\u003c\/td\u003e\n\u003ctd\u003e0.8\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e1.2\u003c\/td\u003e\n\u003ctd\u003e8\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.75\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.8x50N10\u003c\/td\u003e\n\u003ctd\u003e0.8\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e1.2\u003c\/td\u003e\n\u003ctd\u003e10\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.75\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.8x50N12\u003c\/td\u003e\n\u003ctd\u003e0.8\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e1.2\u003c\/td\u003e\n\u003ctd\u003e12\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.75\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.9x50\u003c\/td\u003e\n\u003ctd\u003e0.9\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e1.4\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.85\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.9x50N6\u003c\/td\u003e\n\u003ctd\u003e0.9\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e1.4\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.85\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.9x50N8\u003c\/td\u003e\n\u003ctd\u003e0.9\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e8\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.9x50N10\u003c\/td\u003e\n\u003ctd\u003e0.9\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e1.4\u003c\/td\u003e\n\u003ctd\u003e10\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.85\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-0.9x50N15\u003c\/td\u003e\n\u003ctd\u003e0.9\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e1.4\u003c\/td\u003e\n\u003ctd\u003e15\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.85\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1x50\u003c\/td\u003e\n\u003ctd\u003e1\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.9\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1x50N6\u003c\/td\u003e\n\u003ctd\u003e1\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.9\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1x50N8\u003c\/td\u003e\n\u003ctd\u003e1\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e8\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1x50N10\u003c\/td\u003e\n\u003ctd\u003e1\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e10\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.9\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1x50N12\u003c\/td\u003e\n\u003ctd\u003e1\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e12\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.9\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1x50N14\u003c\/td\u003e\n\u003ctd\u003e1\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e14\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.9\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1x50N16\u003c\/td\u003e\n\u003ctd\u003e1\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e16\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e0.9\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.2x50\u003c\/td\u003e\n\u003ctd\u003e1.2\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e1.8\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.1\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.2x50N6\u003c\/td\u003e\n\u003ctd\u003e1.2\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e1.8\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.1\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.2x50N8\u003c\/td\u003e\n\u003ctd\u003e1.2\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e1.8\u003c\/td\u003e\n\u003ctd\u003e8\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.1\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.2x50N10\u003c\/td\u003e\n\u003ctd\u003e1.2\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e1.8\u003c\/td\u003e\n\u003ctd\u003e10\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.1\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.2x50N12\u003c\/td\u003e\n\u003ctd\u003e1.2\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e1.8\u003c\/td\u003e\n\u003ctd\u003e12\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.1\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.4x50\u003c\/td\u003e\n\u003ctd\u003e1.4\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e2.1\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.3\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.4x50N6\u003c\/td\u003e\n\u003ctd\u003e1.4\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e2.1\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.3\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.4x50N8\u003c\/td\u003e\n\u003ctd\u003e1.4\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e2.1\u003c\/td\u003e\n\u003ctd\u003e8\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.3\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.4x50N10\u003c\/td\u003e\n\u003ctd\u003e1.4\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e2.1\u003c\/td\u003e\n\u003ctd\u003e10\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.3\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.4x50N12\u003c\/td\u003e\n\u003ctd\u003e1.4\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e2.1\u003c\/td\u003e\n\u003ctd\u003e12\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.3\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.4x50N14\u003c\/td\u003e\n\u003ctd\u003e1.4\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e2.1\u003c\/td\u003e\n\u003ctd\u003e14\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.3\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.4x50N16\u003c\/td\u003e\n\u003ctd\u003e1.4\u003c\/td\u003e\n\u003ctd\u003e0.1\u003c\/td\u003e\n\u003ctd\u003e2.1\u003c\/td\u003e\n\u003ctd\u003e16\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.3\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.5x50\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.1\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.4\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.5x50N6\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.3\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.4\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.5x50N8\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.3\u003c\/td\u003e\n\u003ctd\u003e8\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.4\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.5x50N10\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.3\u003c\/td\u003e\n\u003ctd\u003e10\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.4\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.5x50N12\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.3\u003c\/td\u003e\n\u003ctd\u003e12\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.4\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.5x50N14\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.3\u003c\/td\u003e\n\u003ctd\u003e14\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.4\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.5x50N16\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.3\u003c\/td\u003e\n\u003ctd\u003e16\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.4\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.5x60\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.3\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e60\u003c\/td\u003e\n\u003ctd\u003e1.4\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.5x60N18\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.3\u003c\/td\u003e\n\u003ctd\u003e18\u003c\/td\u003e\n\u003ctd\u003e60\u003c\/td\u003e\n\u003ctd\u003e1.4\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.5x60N20\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.3\u003c\/td\u003e\n\u003ctd\u003e20\u003c\/td\u003e\n\u003ctd\u003e60\u003c\/td\u003e\n\u003ctd\u003e1.4\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.6x50\u003c\/td\u003e\n\u003ctd\u003e1.6\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.4\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.6x50N6\u003c\/td\u003e\n\u003ctd\u003e1.6\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.4\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.6x50N8\u003c\/td\u003e\n\u003ctd\u003e1.6\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.4\u003c\/td\u003e\n\u003ctd\u003e8\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.6x50N10\u003c\/td\u003e\n\u003ctd\u003e1.6\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.4\u003c\/td\u003e\n\u003ctd\u003e10\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.6x50N12\u003c\/td\u003e\n\u003ctd\u003e1.6\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.4\u003c\/td\u003e\n\u003ctd\u003e12\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.6x50N14\u003c\/td\u003e\n\u003ctd\u003e1.6\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.4\u003c\/td\u003e\n\u003ctd\u003e14\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.6x50N16\u003c\/td\u003e\n\u003ctd\u003e1.6\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.4\u003c\/td\u003e\n\u003ctd\u003e16\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.6x60\u003c\/td\u003e\n\u003ctd\u003e1.6\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.4\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e60\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.6x60N18\u003c\/td\u003e\n\u003ctd\u003e1.6\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.4\u003c\/td\u003e\n\u003ctd\u003e18\u003c\/td\u003e\n\u003ctd\u003e60\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.6x60N20\u003c\/td\u003e\n\u003ctd\u003e1.6\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.4\u003c\/td\u003e\n\u003ctd\u003e20\u003c\/td\u003e\n\u003ctd\u003e60\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.8x50\u003c\/td\u003e\n\u003ctd\u003e1.8\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.7\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.7\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.8x50N6\u003c\/td\u003e\n\u003ctd\u003e1.8\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.7\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.7\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.8x50N8\u003c\/td\u003e\n\u003ctd\u003e1.8\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.7\u003c\/td\u003e\n\u003ctd\u003e8\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.7\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.8x50N10\u003c\/td\u003e\n\u003ctd\u003e1.8\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.7\u003c\/td\u003e\n\u003ctd\u003e10\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.7\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.8x50N12\u003c\/td\u003e\n\u003ctd\u003e1.8\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.7\u003c\/td\u003e\n\u003ctd\u003e12\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.7\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.8x50N14\u003c\/td\u003e\n\u003ctd\u003e1.8\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.7\u003c\/td\u003e\n\u003ctd\u003e14\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.7\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.8x50N16\u003c\/td\u003e\n\u003ctd\u003e1.8\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.7\u003c\/td\u003e\n\u003ctd\u003e16\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.7\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.8x60\u003c\/td\u003e\n\u003ctd\u003e1.8\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.7\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e60\u003c\/td\u003e\n\u003ctd\u003e1.7\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.8x60N18\u003c\/td\u003e\n\u003ctd\u003e1.8\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e2.7\u003c\/td\u003e\n\u003ctd\u003e18\u003c\/td\u003e\n\u003ctd\u003e60\u003c\/td\u003e\n\u003ctd\u003e1.7\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-1.8x60N20\u003c\/td\u003e\n\u003ctd\u003e1.8\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e20\u003c\/td\u003e\n\u003ctd\u003e60\u003c\/td\u003e\n\u003ctd\u003e1.7\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-2x50\u003c\/td\u003e\n\u003ctd\u003e2\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.9\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-2x50N6\u003c\/td\u003e\n\u003ctd\u003e2\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.9\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-2x50N8\u003c\/td\u003e\n\u003ctd\u003e2\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e8\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.9\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-2x50N10\u003c\/td\u003e\n\u003ctd\u003e2\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e10\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.9\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-2x50N12\u003c\/td\u003e\n\u003ctd\u003e2\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e12\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.9\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-2x50N14\u003c\/td\u003e\n\u003ctd\u003e2\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e14\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.9\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-2x50N16\u003c\/td\u003e\n\u003ctd\u003e2\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e16\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e1.9\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-2x60\u003c\/td\u003e\n\u003ctd\u003e2\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e60\u003c\/td\u003e\n\u003ctd\u003e1.9\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-2x60N18\u003c\/td\u003e\n\u003ctd\u003e2\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e18\u003c\/td\u003e\n\u003ctd\u003e60\u003c\/td\u003e\n\u003ctd\u003e1.9\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-2x60N20\u003c\/td\u003e\n\u003ctd\u003e2\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e20\u003c\/td\u003e\n\u003ctd\u003e60\u003c\/td\u003e\n\u003ctd\u003e1.9\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-2x75\u003c\/td\u003e\n\u003ctd\u003e2\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e75\u003c\/td\u003e\n\u003ctd\u003e1.9\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-2x75N25\u003c\/td\u003e\n\u003ctd\u003e2\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e25\u003c\/td\u003e\n\u003ctd\u003e75\u003c\/td\u003e\n\u003ctd\u003e1.9\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-2x75N30\u003c\/td\u003e\n\u003ctd\u003e2\u003c\/td\u003e\n\u003ctd\u003e0.2\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e30\u003c\/td\u003e\n\u003ctd\u003e75\u003c\/td\u003e\n\u003ctd\u003e1.9\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-2.5x50\u003c\/td\u003e\n\u003ctd\u003e2.5\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e2.4\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-2.5x50N8\u003c\/td\u003e\n\u003ctd\u003e2.5\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e3.7\u003c\/td\u003e\n\u003ctd\u003e8\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e2.4\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-2.5x50N10\u003c\/td\u003e\n\u003ctd\u003e2.5\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e3.7\u003c\/td\u003e\n\u003ctd\u003e10\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e2.4\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-2.5x50N12\u003c\/td\u003e\n\u003ctd\u003e2.5\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e3.7\u003c\/td\u003e\n\u003ctd\u003e12\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e2.4\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-2.5x50N14\u003c\/td\u003e\n\u003ctd\u003e2.5\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e3.7\u003c\/td\u003e\n\u003ctd\u003e14\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e2.4\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-2.5x50N16\u003c\/td\u003e\n\u003ctd\u003e2.5\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e3.7\u003c\/td\u003e\n\u003ctd\u003e16\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e2.4\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-2.5x60\u003c\/td\u003e\n\u003ctd\u003e2.5\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e3.7\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e60\u003c\/td\u003e\n\u003ctd\u003e2.4\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-2.5x60N18\u003c\/td\u003e\n\u003ctd\u003e2.5\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e3.7\u003c\/td\u003e\n\u003ctd\u003e18\u003c\/td\u003e\n\u003ctd\u003e60\u003c\/td\u003e\n\u003ctd\u003e2.4\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-2.5x60N20\u003c\/td\u003e\n\u003ctd\u003e2.5\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e3.7\u003c\/td\u003e\n\u003ctd\u003e20\u003c\/td\u003e\n\u003ctd\u003e60\u003c\/td\u003e\n\u003ctd\u003e2.4\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-2.5x60N25\u003c\/td\u003e\n\u003ctd\u003e2.5\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e3.7\u003c\/td\u003e\n\u003ctd\u003e25\u003c\/td\u003e\n\u003ctd\u003e60\u003c\/td\u003e\n\u003ctd\u003e2.4\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-2.5x75\u003c\/td\u003e\n\u003ctd\u003e2.5\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e3.7\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e75\u003c\/td\u003e\n\u003ctd\u003e2.4\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-2.5x75N30\u003c\/td\u003e\n\u003ctd\u003e2.5\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e30\u003c\/td\u003e\n\u003ctd\u003e75\u003c\/td\u003e\n\u003ctd\u003e2.4\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-3x50\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e2.8\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-3x50N8\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e8\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e2.8\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-3x50N10\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e10\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e2.8\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-3x50N12\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e12\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e2.8\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-3x50N14\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e4.5\u003c\/td\u003e\n\u003ctd\u003e14\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e2.8\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-3x60\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e4.5\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e60\u003c\/td\u003e\n\u003ctd\u003e2.8\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-3x60N16\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e4.5\u003c\/td\u003e\n\u003ctd\u003e16\u003c\/td\u003e\n\u003ctd\u003e60\u003c\/td\u003e\n\u003ctd\u003e2.8\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-3x60N18\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e4.5\u003c\/td\u003e\n\u003ctd\u003e18\u003c\/td\u003e\n\u003ctd\u003e60\u003c\/td\u003e\n\u003ctd\u003e2.8\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-3x60N20\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e4.5\u003c\/td\u003e\n\u003ctd\u003e20\u003c\/td\u003e\n\u003ctd\u003e60\u003c\/td\u003e\n\u003ctd\u003e2.8\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-3x75\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e4.5\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e75\u003c\/td\u003e\n\u003ctd\u003e2.8\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-3x75N25\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e4.5\u003c\/td\u003e\n\u003ctd\u003e25\u003c\/td\u003e\n\u003ctd\u003e75\u003c\/td\u003e\n\u003ctd\u003e2.8\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-4x60\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003ctd\u003e0.4\u003c\/td\u003e\n\u003ctd\u003e4.5\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e60\u003c\/td\u003e\n\u003ctd\u003e3.7\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-4x60N10\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003ctd\u003e0.4\u003c\/td\u003e\n\u003ctd\u003e4.5\u003c\/td\u003e\n\u003ctd\u003e10\u003c\/td\u003e\n\u003ctd\u003e60\u003c\/td\u003e\n\u003ctd\u003e3.7\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-4x60N15\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003ctd\u003e0.4\u003c\/td\u003e\n\u003ctd\u003e4.5\u003c\/td\u003e\n\u003ctd\u003e15\u003c\/td\u003e\n\u003ctd\u003e60\u003c\/td\u003e\n\u003ctd\u003e3.7\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-4x60N20\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003ctd\u003e0.4\u003c\/td\u003e\n\u003ctd\u003e4.5\u003c\/td\u003e\n\u003ctd\u003e20\u003c\/td\u003e\n\u003ctd\u003e60\u003c\/td\u003e\n\u003ctd\u003e3.7\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-4x75\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003ctd\u003e0.4\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e75\u003c\/td\u003e\n\u003ctd\u003e3.7\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-4x75N25\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003ctd\u003e0.4\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e25\u003c\/td\u003e\n\u003ctd\u003e75\u003c\/td\u003e\n\u003ctd\u003e3.7\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-4x75N30\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003ctd\u003e0.4\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e30\u003c\/td\u003e\n\u003ctd\u003e75\u003c\/td\u003e\n\u003ctd\u003e3.7\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22C-4x75N40\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003ctd\u003e0.4\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e40\u003c\/td\u003e\n\u003ctd\u003e75\u003c\/td\u003e\n\u003ctd\u003e3.7\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22U-0.3N2\u003c\/td\u003e\n\u003ctd\u003e0.3\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e2\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22U-1N6\u003c\/td\u003e\n\u003ctd\u003e1\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22U-1.5N6\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22U-1.5N8\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e8\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22U-1.5N12\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e12\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22U-1.5N16\u003c\/td\u003e\n\u003ctd\u003e1.5\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e16\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22U-2N12\u003c\/td\u003e\n\u003ctd\u003e2\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e12\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22U-2N16\u003c\/td\u003e\n\u003ctd\u003e2\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e16\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22U-2N20\u003c\/td\u003e\n\u003ctd\u003e2\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e20\u003c\/td\u003e\n\u003ctd\u003e60\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22U-3N10\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e10\u003c\/td\u003e\n\u003ctd\u003e50\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22U-3N16\u003c\/td\u003e\n\u003ctd\u003e3\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e16\u003c\/td\u003e\n\u003ctd\u003e60\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr\u003e\n\u003ctd\u003eLL-ST22U-4N15\u003c\/td\u003e\n\u003ctd\u003e4\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e15\u003c\/td\u003e\n\u003ctd\u003e60\u003c\/td\u003e\n\u003ctd\u003e\u003c\/td\u003e\n\u003ctd\u003e6\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003c\/table\u003e\u003c\/div\u003e\u003cp\u003e\u003cem\u003eDimensions are confirmed on each quotation.\u003c\/em\u003e\u003c\/p\u003e\u003ch4\u003eNeed a special tool design?\u003c\/h4\u003e\u003cp\u003eSpeak to us. We design and supply special diameters, lengths, corner radii, profiles and step tools. Send a drawing or a sketch to \u003ca href=\"mailto:info@latheland.com\"\u003einfo@latheland.com\u003c\/a\u003e or call +44 7727 992812.\u003c\/p\u003e\u003cp\u003e\u003cstrong\u003eLATHELAND®\u003c\/strong\u003e\u003c\/p\u003e","brand":"LATHELAND","offers":[{"title":"ST22C – AlCrN \/ Ø0.2 · L50","offer_id":54915208282458,"sku":"LL-ST22C-0.2x50","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.2 · L50 · reach 0.5","offer_id":54915208315226,"sku":"LL-ST22C-0.2x50N0.5","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.2 · L50 · reach 1","offer_id":54915208347994,"sku":"LL-ST22C-0.2x50N1","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.2 · L50 · reach 1.5","offer_id":54915208380762,"sku":"LL-ST22C-0.2x50N1.5","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.3 · L50","offer_id":54915208413530,"sku":"LL-ST22C-0.3x50","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.3 · L50 · reach 1","offer_id":54915208446298,"sku":"LL-ST22C-0.3x50N1","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.3 · L50 · reach 2","offer_id":54915208479066,"sku":"LL-ST22C-0.3x50N2","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.3 · L50 · reach 3","offer_id":54915208511834,"sku":"LL-ST22C-0.3x50N3","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.4 · L50","offer_id":54915208544602,"sku":"LL-ST22C-0.4x50","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.4 · L50 · reach 2","offer_id":54915208577370,"sku":"LL-ST22C-0.4x50N2","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.4 · L50 · reach 3","offer_id":54915208610138,"sku":"LL-ST22C-0.4x50N3","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.4 · L50 · reach 4","offer_id":54915208642906,"sku":"LL-ST22C-0.4x50N4","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.4 · L50 · reach 5","offer_id":54915208675674,"sku":"LL-ST22C-0.4x50N5","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.5 · L50","offer_id":54915208708442,"sku":"LL-ST22C-0.5x50","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.5 · L50 · reach 2","offer_id":54915208741210,"sku":"LL-ST22C-0.5x50N2","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.5 · L50 · reach 4","offer_id":54915208773978,"sku":"LL-ST22C-0.5x50N4","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.5 · L50 · reach 6","offer_id":54915208806746,"sku":"LL-ST22C-0.5x50N6","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.5 · L50 · reach 8","offer_id":54915208839514,"sku":"LL-ST22C-0.5x50N8","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.6 · L50","offer_id":54915208872282,"sku":"LL-ST22C-0.6x50","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.6 · L50 · reach 2","offer_id":54915208905050,"sku":"LL-ST22C-0.6x50N2","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.6 · L50 · reach 4","offer_id":54915208937818,"sku":"LL-ST22C-0.6x50N4","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.6 · L50 · reach 6","offer_id":54915208970586,"sku":"LL-ST22C-0.6x50N6","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.6 · L50 · reach 8","offer_id":54915209003354,"sku":"LL-ST22C-0.6x50N8","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.6 · L50 · reach 10","offer_id":54915209036122,"sku":"LL-ST22C-0.6x50N10","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.7 · L50","offer_id":54915209068890,"sku":"LL-ST22C-0.7x50","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.7 · L50 · reach 2","offer_id":54915209101658,"sku":"LL-ST22C-0.7x50N2","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.7 · L50 · reach 4","offer_id":54915209134426,"sku":"LL-ST22C-0.7x50N4","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.7 · L50 · reach 6","offer_id":54915209167194,"sku":"LL-ST22C-0.7x50N6","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.7 · L50 · reach 8","offer_id":54915209199962,"sku":"LL-ST22C-0.7x50N8","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.7 · L50 · reach 10","offer_id":54915209232730,"sku":"LL-ST22C-0.7x50N10","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.8 · L50","offer_id":54915209265498,"sku":"LL-ST22C-0.8x50","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.8 · L50 · reach 4","offer_id":54915209298266,"sku":"LL-ST22C-0.8x50N4","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.8 · L50 · reach 6","offer_id":54915209331034,"sku":"LL-ST22C-0.8x50N6","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.8 · L50 · reach 8","offer_id":54915209363802,"sku":"LL-ST22C-0.8x50N8","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.8 · L50 · reach 10","offer_id":54915209396570,"sku":"LL-ST22C-0.8x50N10","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.8 · L50 · reach 12","offer_id":54915209429338,"sku":"LL-ST22C-0.8x50N12","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.9 · L50","offer_id":54915209462106,"sku":"LL-ST22C-0.9x50","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.9 · L50 · reach 6","offer_id":54915209494874,"sku":"LL-ST22C-0.9x50N6","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.9 · L50 · reach 8","offer_id":54915209527642,"sku":"LL-ST22C-0.9x50N8","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.9 · L50 · reach 10","offer_id":54915209560410,"sku":"LL-ST22C-0.9x50N10","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø0.9 · L50 · reach 15","offer_id":54915209593178,"sku":"LL-ST22C-0.9x50N15","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1 · L50","offer_id":54915209625946,"sku":"LL-ST22C-1x50","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1 · L50 · reach 6","offer_id":54915209658714,"sku":"LL-ST22C-1x50N6","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1 · L50 · reach 8","offer_id":54915209691482,"sku":"LL-ST22C-1x50N8","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1 · L50 · reach 10","offer_id":54915209724250,"sku":"LL-ST22C-1x50N10","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1 · L50 · reach 12","offer_id":54915209757018,"sku":"LL-ST22C-1x50N12","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1 · L50 · reach 14","offer_id":54915209789786,"sku":"LL-ST22C-1x50N14","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1 · L50 · reach 16","offer_id":54915209822554,"sku":"LL-ST22C-1x50N16","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.2 · L50","offer_id":54915209855322,"sku":"LL-ST22C-1.2x50","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.2 · L50 · reach 6","offer_id":54915209888090,"sku":"LL-ST22C-1.2x50N6","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.2 · L50 · reach 8","offer_id":54915209920858,"sku":"LL-ST22C-1.2x50N8","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.2 · L50 · reach 10","offer_id":54915209953626,"sku":"LL-ST22C-1.2x50N10","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.2 · L50 · reach 12","offer_id":54915209986394,"sku":"LL-ST22C-1.2x50N12","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.4 · L50","offer_id":54915210019162,"sku":"LL-ST22C-1.4x50","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.4 · L50 · reach 6","offer_id":54915210051930,"sku":"LL-ST22C-1.4x50N6","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.4 · L50 · reach 8","offer_id":54915210084698,"sku":"LL-ST22C-1.4x50N8","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.4 · L50 · reach 10","offer_id":54915210117466,"sku":"LL-ST22C-1.4x50N10","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.4 · L50 · reach 12","offer_id":54915210150234,"sku":"LL-ST22C-1.4x50N12","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.4 · L50 · reach 14","offer_id":54915210183002,"sku":"LL-ST22C-1.4x50N14","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.4 · L50 · reach 16","offer_id":54915210215770,"sku":"LL-ST22C-1.4x50N16","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.5 · L50","offer_id":54915210248538,"sku":"LL-ST22C-1.5x50","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.5 · L50 · reach 6","offer_id":54915210281306,"sku":"LL-ST22C-1.5x50N6","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.5 · L50 · reach 8","offer_id":54915210314074,"sku":"LL-ST22C-1.5x50N8","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.5 · L50 · reach 10","offer_id":54915210346842,"sku":"LL-ST22C-1.5x50N10","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.5 · L50 · reach 12","offer_id":54915210379610,"sku":"LL-ST22C-1.5x50N12","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.5 · L50 · reach 14","offer_id":54915210412378,"sku":"LL-ST22C-1.5x50N14","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.5 · L50 · reach 16","offer_id":54915210445146,"sku":"LL-ST22C-1.5x50N16","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.5 · L60","offer_id":54915210477914,"sku":"LL-ST22C-1.5x60","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.5 · L60 · reach 18","offer_id":54915210510682,"sku":"LL-ST22C-1.5x60N18","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.5 · L60 · reach 20","offer_id":54915210543450,"sku":"LL-ST22C-1.5x60N20","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.6 · L50","offer_id":54915210576218,"sku":"LL-ST22C-1.6x50","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.6 · L50 · reach 6","offer_id":54915210608986,"sku":"LL-ST22C-1.6x50N6","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.6 · L50 · reach 8","offer_id":54915210641754,"sku":"LL-ST22C-1.6x50N8","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.6 · L50 · reach 10","offer_id":54915210674522,"sku":"LL-ST22C-1.6x50N10","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.6 · L50 · reach 12","offer_id":54915210707290,"sku":"LL-ST22C-1.6x50N12","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.6 · L50 · reach 14","offer_id":54915210740058,"sku":"LL-ST22C-1.6x50N14","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.6 · L50 · reach 16","offer_id":54915210772826,"sku":"LL-ST22C-1.6x50N16","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.6 · L60","offer_id":54915210805594,"sku":"LL-ST22C-1.6x60","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.6 · L60 · reach 18","offer_id":54915210838362,"sku":"LL-ST22C-1.6x60N18","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.6 · L60 · reach 20","offer_id":54915210871130,"sku":"LL-ST22C-1.6x60N20","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.8 · L50","offer_id":54915210903898,"sku":"LL-ST22C-1.8x50","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.8 · L50 · reach 6","offer_id":54915210936666,"sku":"LL-ST22C-1.8x50N6","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.8 · L50 · reach 8","offer_id":54915210969434,"sku":"LL-ST22C-1.8x50N8","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.8 · L50 · reach 10","offer_id":54915211002202,"sku":"LL-ST22C-1.8x50N10","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.8 · L50 · reach 12","offer_id":54915211034970,"sku":"LL-ST22C-1.8x50N12","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.8 · L50 · reach 14","offer_id":54915211067738,"sku":"LL-ST22C-1.8x50N14","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.8 · L50 · reach 16","offer_id":54915211100506,"sku":"LL-ST22C-1.8x50N16","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.8 · L60","offer_id":54915211133274,"sku":"LL-ST22C-1.8x60","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.8 · L60 · reach 18","offer_id":54915211166042,"sku":"LL-ST22C-1.8x60N18","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø1.8 · L60 · reach 20","offer_id":54915211198810,"sku":"LL-ST22C-1.8x60N20","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø2 · L50","offer_id":54915211231578,"sku":"LL-ST22C-2x50","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø2 · L50 · reach 6","offer_id":54915211264346,"sku":"LL-ST22C-2x50N6","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø2 · L50 · reach 8","offer_id":54915211297114,"sku":"LL-ST22C-2x50N8","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø2 · L50 · reach 10","offer_id":54915211329882,"sku":"LL-ST22C-2x50N10","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø2 · L50 · reach 12","offer_id":54915211362650,"sku":"LL-ST22C-2x50N12","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø2 · L50 · reach 14","offer_id":54915211395418,"sku":"LL-ST22C-2x50N14","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø2 · L50 · reach 16","offer_id":54915211428186,"sku":"LL-ST22C-2x50N16","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø2 · L60","offer_id":54915211460954,"sku":"LL-ST22C-2x60","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø2 · L60 · reach 18","offer_id":54915211493722,"sku":"LL-ST22C-2x60N18","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø2 · L60 · reach 20","offer_id":54915211526490,"sku":"LL-ST22C-2x60N20","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø2 · L75","offer_id":54915211559258,"sku":"LL-ST22C-2x75","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø2 · L75 · reach 25","offer_id":54915211592026,"sku":"LL-ST22C-2x75N25","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø2 · L75 · reach 30","offer_id":54915211624794,"sku":"LL-ST22C-2x75N30","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø2.5 · L50","offer_id":54915211657562,"sku":"LL-ST22C-2.5x50","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø2.5 · L50 · reach 8","offer_id":54915211690330,"sku":"LL-ST22C-2.5x50N8","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø2.5 · L50 · reach 10","offer_id":54915211723098,"sku":"LL-ST22C-2.5x50N10","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø2.5 · L50 · reach 12","offer_id":54915211755866,"sku":"LL-ST22C-2.5x50N12","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø2.5 · L50 · reach 14","offer_id":54915211788634,"sku":"LL-ST22C-2.5x50N14","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø2.5 · L50 · reach 16","offer_id":54915211821402,"sku":"LL-ST22C-2.5x50N16","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø2.5 · L60","offer_id":54915211854170,"sku":"LL-ST22C-2.5x60","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø2.5 · L60 · reach 18","offer_id":54915211886938,"sku":"LL-ST22C-2.5x60N18","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø2.5 · L60 · reach 20","offer_id":54915211919706,"sku":"LL-ST22C-2.5x60N20","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø2.5 · L60 · reach 25","offer_id":54915211952474,"sku":"LL-ST22C-2.5x60N25","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø2.5 · L75","offer_id":54915211985242,"sku":"LL-ST22C-2.5x75","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø2.5 · L75 · reach 30","offer_id":54915212018010,"sku":"LL-ST22C-2.5x75N30","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø3 · L50","offer_id":54915212050778,"sku":"LL-ST22C-3x50","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø3 · L50 · reach 8","offer_id":54915212083546,"sku":"LL-ST22C-3x50N8","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø3 · L50 · reach 10","offer_id":54915212116314,"sku":"LL-ST22C-3x50N10","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø3 · L50 · reach 12","offer_id":54915212149082,"sku":"LL-ST22C-3x50N12","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø3 · L50 · reach 14","offer_id":54915212181850,"sku":"LL-ST22C-3x50N14","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø3 · L60","offer_id":54915212214618,"sku":"LL-ST22C-3x60","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø3 · L60 · reach 16","offer_id":54915212247386,"sku":"LL-ST22C-3x60N16","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø3 · L60 · reach 18","offer_id":54915212280154,"sku":"LL-ST22C-3x60N18","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø3 · L60 · reach 20","offer_id":54915212312922,"sku":"LL-ST22C-3x60N20","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø3 · L75","offer_id":54915212345690,"sku":"LL-ST22C-3x75","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø3 · L75 · reach 25","offer_id":54915212378458,"sku":"LL-ST22C-3x75N25","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø4 · L60","offer_id":54915212411226,"sku":"LL-ST22C-4x60","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø4 · L60 · reach 10","offer_id":54915212443994,"sku":"LL-ST22C-4x60N10","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø4 · L60 · reach 15","offer_id":54915212476762,"sku":"LL-ST22C-4x60N15","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø4 · L60 · reach 20","offer_id":54915212509530,"sku":"LL-ST22C-4x60N20","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø4 · L75","offer_id":54915212542298,"sku":"LL-ST22C-4x75","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø4 · L75 · reach 25","offer_id":54915212575066,"sku":"LL-ST22C-4x75N25","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø4 · L75 · reach 30","offer_id":54915212607834,"sku":"LL-ST22C-4x75N30","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22C – AlCrN \/ Ø4 · L75 · reach 40","offer_id":54915212640602,"sku":"LL-ST22C-4x75N40","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22U – Uncoated, polished \/ Ø0.3 · reach 2","offer_id":54915212673370,"sku":"LL-ST22U-0.3N2","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22U – Uncoated, polished \/ Ø1 · reach 6","offer_id":54915212706138,"sku":"LL-ST22U-1N6","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22U – Uncoated, polished \/ Ø1.5 · reach 6","offer_id":54915212738906,"sku":"LL-ST22U-1.5N6","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22U – Uncoated, polished \/ Ø1.5 · reach 8","offer_id":54915212771674,"sku":"LL-ST22U-1.5N8","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22U – Uncoated, polished \/ Ø1.5 · reach 12","offer_id":54915212804442,"sku":"LL-ST22U-1.5N12","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22U – Uncoated, polished \/ Ø1.5 · reach 16","offer_id":54915212837210,"sku":"LL-ST22U-1.5N16","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22U – Uncoated, polished \/ Ø2 · reach 12","offer_id":54915212869978,"sku":"LL-ST22U-2N12","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22U – Uncoated, polished \/ Ø2 · reach 16","offer_id":54915212902746,"sku":"LL-ST22U-2N16","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22U – Uncoated, polished \/ Ø2 · reach 20","offer_id":54915212935514,"sku":"LL-ST22U-2N20","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22U – Uncoated, polished \/ Ø3 · reach 10","offer_id":54915212968282,"sku":"LL-ST22U-3N10","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22U – Uncoated, polished \/ Ø3 · reach 16","offer_id":54915213001050,"sku":"LL-ST22U-3N16","price":0.0,"currency_code":"GBP","in_stock":false},{"title":"ST22U – Uncoated, polished \/ Ø4 · reach 15","offer_id":54915213033818,"sku":"LL-ST22U-4N15","price":0.0,"currency_code":"GBP","in_stock":false}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0924\/6795\/4010\/files\/latheland-range-st22-marked.jpg?v=1791295559","url":"https:\/\/www.latheland.co.uk\/products\/latheland-range-st22-miniature-torus-end-mill-with-long-neck-for-stainless-titanium-superalloys-2-4-flutes","provider":"LATHELAND","version":"1.0","type":"link"}